CURING:
Following procedure should be adopted for curing
PCC sprinkling of water
FOOTING should be covered by wet gunny bags intermediate sprinkling of water
COLUMN should be covered by wet gunny bags
BEAM should be covered by wet gunny bags sprinkling of water bottom side after de- shuttering
SLAB water ponding of minimum 2" depth & maximum size between 6' X 6' ponding size
BRICK WORK intermittent sprinkling of water
INTERNAL&
EXTERNAL intermittent sprinkling PLASTERING of water
WATER PROOFING By bonding
TILING Intermittent sprinkling of water
EXTERNAL intermittent sprinkling PAINTING of water